Sipolprene SP 215 LV

High-modulus TPC-ET at Shore D 65 and MFI 35, with a 215 °C melting point and 470 MPa flexural modulus. Natural grade stated FDA and EU 10/2011 compliant.

Home › Products › Sipol › Sipolprene SP 215 LV

Sipolprene SP 215 LV is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 65, with a 215 °C melting point and a melt flow of 35 g/10 min at 230 °C, 2.16 kg. Sipol designed it as a high-modulus ether ester elastomer with a rheology suited to injection molding and extrusion.

The natural grade carries Sipol's standard stabilization package and, per Sipol's data sheet, is in compliance with American FDA and European EU 10/2011 food contact regulations.

Its typical properties match Sipolprene 65215 row for row except melt flow, which is 35 g/10 min here against 21. That higher flow is the low-viscosity (LV) position: the same Shore D 65 part, with easier filling of long flow paths and thin sections in the mold.

Flexural modulus is 470 MPa, stress at break 52 MPa and elongation at break 500 percent. The 215 °C melt and 203 °C Vicat A/50 set the upper limit for heat exposure, and the glass transition sits at 16 °C.

Notched Izod is no break at 23 °C and 20 J/m at -40 °C (ISO 180), and abrasion loss is 55 mm³. Sipol has no separate data sheet for an SP 215 LV version; black, UV-stabilized and heat-stabilized dry blends are available on request.

It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.

Typical properties

PropertyTypical value
Melting temperature215 °C (ISO 11357-3)
Crystallization temperature178 °C (ISO 11357-3)
Glass transition temperature16 °C (ISO 11357-2)
Vicat softening temperature A/50203 °C (ISO 306)
Melt flow index (MFI)35 g/10 min at 230 °C, 2.16 kg (ISO 1133)
Melt volume rate (MVR)28 cm³/10 min at 230 °C, 2.16 kg (ISO 1133)
Shore D hardness65 instantaneous, 62 after 15 s (ISO 868)
Stress at break52 MPa (ISO 527)
Elongation at break500 % (ISO 527)
Flexural modulus470 MPa (ISO 178)
Notched Izod impact at 23 °CNo break (ISO 180)
Notched Izod impact at -40 °C20 J/m (ISO 180)
Abrasion loss55 mm³ at 5 N vertical load (ISO 4649)
Density1.23 g/cm³ (ISO 1183)
Water absorption0.2 % after 24 h immersion at 23 °C (Sipol method MI 08)
ColorNatural
FormGranules
VersionsBlack, UV-stabilized and heat-stabilized dry blends on request

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Injection molded parts

At MFI 35 g/10 min it fills the mold more easily than 65215, on a profile of 200 °C at the rear zone up to 225 °C at the nozzle.

Extruded parts

Sipol's extrusion profile climbs from 195 to 210 °C at the feed to 210 to 225 °C at the head and die.

Food-contact parts

The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.

Black, UV and heat-stabilized parts

Sipol supplies black, UV-stabilized and heat-stabilized dry blends on request.

Handling and dispersion

Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.

For injection molding, Sipol suggests the rear zone at 200 °C, the center zone at 210 °C, the front zone at 220 °C and the nozzle at 225 °C, with the mold at 30 to 40 °C.

For extrusion, the suggested profile is feed zone 195 to 210 °C, compression zone 210 to 220 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C.

Packaging, storage, and regulatory status

Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..

Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.

Sipol states the natural grade is in compliance with American FDA and European EU 10/2011 food contact regulations. Read the safety data sheet before handling.

Frequently asked questions

What separates Sipolprene SP 215 LV from Sipolprene 65215?

Melt flow is the only difference between Sipolprene SP 215 LV and 65215 on Sipol's sheets. SP 215 LV runs at MFI 35 g/10 min and MVR 28 cm³/10 min, against MFI 21 and MVR 17 for 65215, at 230 °C and 2.16 kg. Shore D 65, the 215 °C melt, 470 MPa flexural modulus, 52 MPa stress at break and every other listed value are the same.

When should I choose Sipolprene SP 215 LV?

Choose Sipolprene SP 215 LV when a Shore D 65 molding has long flow paths or thin walls that 65215 at MFI 21 g/10 min struggles to fill. At MFI 35 g/10 min it reaches the same hardness and 470 MPa stiffness with less injection pressure. Where the part is extruded and needs melt strength, the lower-flow 65215 is the usual starting point.

What processing temperatures does Sipolprene SP 215 LV need?

Sipolprene SP 215 LV melts at 215 °C. For injection molding Sipol suggests 200 °C at the rear zone, 210 °C center, 220 °C front and 225 °C at the nozzle, with the mold at 30 to 40 °C. For extrusion the profile runs 195 to 210 °C at the feed, 210 to 220 °C in compression, and 210 to 225 °C through metering and the die. Dry 2 to 3 hours at 90 °C first.

Is Sipolprene SP 215 LV food-contact compliant?

Sipol's data sheet states that natural Sipolprene SP 215 LV, with its standard stabilization package, is in compliance with American FDA and European EU 10/2011 food contact regulations. Black, UV-stabilized or heat-stabilized dry blends are not covered by that statement on the sheet, so specify the natural grade for a food-contact part and ask for the food contact declaration with the TDS and SDS.

Can I get the TDS and SDS for Sipolprene SP 215 LV?

Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Sipolprene 65215

The same Shore D 65 property set at MFI 21, for extrusion and general molding.

Sipolprene 60212

Shore D 60 high-modulus grade at 460 MPa with 235 N/mm tear.

Sipolprene 68217

Harder at Shore D 68 and 525 MPa, with black and UV versions.

Where this grade fits

TPC-ET copolyester elastomers

The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.

What is TPC-ET

What the TPC-ET name means and how copolyester elastomer differs from TPU.

Matching a TPC-ET specification

Matching an existing specification by Shore D hardness, melt viscosity and version suffix.

Evaluating Sipolprene SP 215 LV?

Tell us the system you are formulating and the property you need to hit. We will confirm the grade, send the data sheet, and ship a sample.