High-modulus TPC-ET at Shore D 68 with a 217 °C melting point, 208 °C Vicat and 525 MPa flexural modulus. Natural grade FDA and EU 10/2011, black and UV versions.

Home › Products › Sipol › Sipolprene 68217

Sipolprene 68217 is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 68, with a 217 °C melting point and a melt flow of 20 g/10 min at 230 °C, 2.16 kg. Sipol designed it as a high-modulus ether ester elastomer with a rheology suited to injection molding and extrusion.

The natural grade carries Sipol's standard stabilization package and, per Sipol's data sheet, is in compliance with American FDA and European EU 10/2011 food contact regulations.

Flexural modulus is 525 MPa and stress at break 58 MPa, with elongation at break still at 490 percent. The 217 °C melt and 208 °C Vicat A/50 suit parts that run hot, and the glass transition sits at 30 °C, above room temperature.

Notched Izod is 37 J/m at 23 °C and 34 J/m at -40 °C (ISO 180), nearly flat across the range, so a notch or sharp corner matters more on this grade than on the softer ones. Compression set is 18 percent at 23 °C and 67 percent at 70 °C, and abrasion loss is 56 mm³.

Three versions have their own Sipol data sheets. 68217 B is a black dry blend, 68217 W a UV-stabilized dry blend and 68217 WB a UV-stabilized black dry blend, all with the natural grade's typical values and processing profile. A heat-stabilized dry blend is available on request.

It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.

Typical properties

PropertyTypical value
Melting temperature217 °C (ISO 11357-3)
Crystallization temperature177 °C (ISO 11357-3)
Glass transition temperature30 °C (ISO 11357-2)
Vicat softening temperature A/50208 °C (ISO 306)
Melt flow index (MFI)20 g/10 min at 230 °C, 2.16 kg (ISO 1133)
Melt volume rate (MVR)16 cm³/10 min at 230 °C, 2.16 kg (ISO 1133)
Shore D hardness68 instantaneous, 65 after 15 s (ISO 868)
Stress at break58 MPa (ISO 527)
Elongation at break490 % (ISO 527)
Flexural modulus525 MPa (ISO 178)
Notched Izod impact at 23 °C37 J/m (ISO 180)
Notched Izod impact at -40 °C34 J/m (ISO 180)
Abrasion loss56 mm³ at 5 N vertical load (ISO 4649)
Compression set at 23 °C18 % (ISO 815:1991)
Compression set at 70 °C67 % (ISO 815:1991)
Density1.25 g/cm³ (ISO 1183)
Water absorption0.2 % after 24 h immersion at 23 °C (Sipol method MI 08)
ColorNatural
FormGranules
Versions68217 B (black dry blend), 68217 W (UV-stabilized dry blend), 68217 WB (UV-stabilized black dry blend)

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Injection molded parts

Sipol's profile runs 195 to 210 °C at the rear zone up to 240 °C at the nozzle, with the mold at 40 to 50 °C.

Extruded parts

The extrusion profile climbs from 200 to 215 °C at the feed to 215 to 230 °C at the head and die.

Food-contact parts

The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.

Black parts

68217 B is the black dry blend.

UV-exposed parts

68217 W is UV-stabilized, and 68217 WB is UV-stabilized and black.

Handling and dispersion

Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.

For injection molding, Sipol suggests the rear zone at 195 to 210 °C, the center zone at 220 °C, the front zone at 230 °C and the nozzle at 240 °C, with a warmer mold at 40 to 50 °C.

For extrusion, the suggested profile is feed zone 200 to 215 °C, compression zone 215 to 225 °C, metering zone 215 to 230 °C and head or die 215 to 230 °C.

Packaging, storage, and regulatory status

Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..

Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.

Sipol states the natural grade is in compliance with American FDA and European EU 10/2011 food contact regulations. Read the safety data sheet before handling.

Frequently asked questions

What processing temperatures does Sipolprene 68217 need?

Sipolprene 68217 melts at 217 °C and runs hotter than the softer Sipolprene grades. For injection molding Sipol suggests 195 to 210 °C at the rear zone, 220 °C center, 230 °C front and 240 °C at the nozzle, with the mold at 40 to 50 °C. For extrusion the profile runs 200 to 215 °C at the feed, 215 to 225 °C in compression, and 215 to 230 °C through metering and the die. Dry 2 to 3 hours at 90 °C first.

How tough is Sipolprene 68217 on impact?

Sipolprene 68217 reads 37 J/m notched Izod at 23 °C and 34 J/m at -40 °C (ISO 180). The small drop from room temperature to -40 °C means cold behavior tracks room-temperature behavior closely, but the notched values are lower than the softer grades. Sipolprene 63210 at Shore D 62 reads 155 J/m and 82 J/m for comparison, so design out sharp notches in a 68217 part.

Is Sipolprene 68217 food-contact compliant?

Sipol's data sheet states that natural Sipolprene 68217 is in compliance with American FDA and European EU 10/2011 food contact regulations. The 68217 B, W and WB dry-blend sheets do not carry that statement, so a food-contact part should be specified in the natural grade. Ask for the food contact declaration with the TDS and SDS.

What separates Sipolprene 68217 from Sipolprene 72220?

Sipolprene 72220 is harder at Shore D 72 against 68 and stiffer at 660 MPa against 525 MPa, with a 218 °C melt against 217 °C. Sipolprene 68217 is stronger at break, 58 MPa against 53 MPa, loses less to abrasion at 56 mm³ against 76 mm³, and carries an FDA and EU 10/2011 food contact statement that the 72220 sheet does not.

Can I get the TDS and SDS for Sipolprene 68217?

Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Sipolprene 72220

Shore D 72 at 660 MPa, with copper deactivation stabilization for hot cable jacketing.

Sipolprene 65215

Shore D 65 at 470 MPa, no break in notched Izod at 23 °C.

Sipolprene 63210

Shore D 62 at 320 MPa, with higher notched impact and an HV extrusion version.

Where this grade fits

TPC-ET copolyester elastomers

The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.

What is TPC-ET

What the TPC-ET name means and how copolyester elastomer differs from TPU.

Matching a TPC-ET specification

Matching an existing specification by Shore D hardness, melt viscosity and version suffix.

Evaluating Sipolprene 68217?

Tell us the system you are formulating and the property you need to hit. We will confirm the grade, send the data sheet, and ship a sample.