Sipolprene 65215

High-modulus TPC-ET at Shore D 65 with a 215 °C melting point, 470 MPa flexural modulus and MFI 21. Natural grade stated FDA and EU 10/2011 compliant.

Home › Products › Sipol › Sipolprene 65215

Sipolprene 65215 is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 65, with a 215 °C melting point and a melt flow of 21 g/10 min at 230 °C, 2.16 kg. Sipol designed it as a high-modulus ether ester elastomer with a rheology suited to injection molding and extrusion.

The natural grade carries Sipol's standard stabilization package and, per Sipol's data sheet, is in compliance with American FDA and European EU 10/2011 food contact regulations.

Flexural modulus is 470 MPa, stress at break 52 MPa and elongation at break 500 percent. The 215 °C melt and 203 °C Vicat A/50 give a part room to work at elevated temperature, and the glass transition sits at 16 °C.

Notched Izod is no break at 23 °C and 20 J/m at -40 °C (ISO 180), so a part that takes impact in deep cold should be tested at its service temperature. Abrasion loss is 55 mm³ (ISO 4649).

Sipol has no separate data sheet for a 65215 version; black, UV-stabilized and heat-stabilized dry blends are available on request. Sipolprene SP 215 LV carries the same typical properties at a higher melt flow of 35 g/10 min.

It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.

Typical properties

PropertyTypical value
Melting temperature215 °C (ISO 11357-3)
Crystallization temperature178 °C (ISO 11357-3)
Glass transition temperature16 °C (ISO 11357-2)
Vicat softening temperature A/50203 °C (ISO 306)
Melt flow index (MFI)21 g/10 min at 230 °C, 2.16 kg (ISO 1133)
Melt volume rate (MVR)17 cm³/10 min at 230 °C, 2.16 kg (ISO 1133)
Shore D hardness65 instantaneous, 62 after 15 s (ISO 868)
Stress at break52 MPa (ISO 527)
Elongation at break500 % (ISO 527)
Flexural modulus470 MPa (ISO 178)
Notched Izod impact at 23 °CNo break (ISO 180)
Notched Izod impact at -40 °C20 J/m (ISO 180)
Abrasion loss55 mm³ at 5 N vertical load (ISO 4649)
Density1.23 g/cm³ (ISO 1183)
Water absorption0.2 % after 24 h immersion at 23 °C (Sipol method MI 08)
ColorNatural
FormGranules
VersionsBlack, UV-stabilized and heat-stabilized dry blends on request

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Injection molded parts

Sipol's profile runs 200 °C at the rear zone up to 225 °C at the nozzle, with the mold at 30 to 40 °C.

Extruded parts

The extrusion profile climbs from 195 to 210 °C at the feed to 210 to 225 °C at the head and die.

Food-contact parts

The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.

Black, UV and heat-stabilized parts

Sipol supplies black, UV-stabilized and heat-stabilized dry blends on request.

Handling and dispersion

Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.

For injection molding, Sipol suggests the rear zone at 200 °C, the center zone at 210 °C, the front zone at 220 °C and the nozzle at 225 °C, with the mold at 30 to 40 °C.

For extrusion, the suggested profile is feed zone 195 to 210 °C, compression zone 210 to 220 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C.

Packaging, storage, and regulatory status

Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..

Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.

Sipol states the natural grade is in compliance with American FDA and European EU 10/2011 food contact regulations. Read the safety data sheet before handling.

Frequently asked questions

What processing temperatures does Sipolprene 65215 need?

Sipolprene 65215 melts at 215 °C. For injection molding Sipol suggests 200 °C at the rear zone, 210 °C center, 220 °C front and 225 °C at the nozzle, with the mold at 30 to 40 °C. For extrusion the profile runs 195 to 210 °C at the feed, 210 to 220 °C in compression, and 210 to 225 °C through metering and the die. Dry first for 2 to 3 hours at 90 °C in a dehumidifying dryer.

What separates Sipolprene 65215 from Sipolprene SP 215 LV?

Melt flow is the only difference between Sipolprene 65215 and SP 215 LV on Sipol's sheets. 65215 runs at MFI 21 g/10 min and SP 215 LV at MFI 35 g/10 min, both at 230 °C and 2.16 kg. Every other listed value matches, including Shore D 65, the 215 °C melting point, 470 MPa flexural modulus and 52 MPa stress at break. SP 215 LV is the low-viscosity choice when a mold needs easier filling.

Is Sipolprene 65215 food-contact compliant?

Sipol's data sheet states that natural Sipolprene 65215, with its standard stabilization package, is in compliance with American FDA and European EU 10/2011 food contact regulations. Black, UV-stabilized or heat-stabilized dry blends are not covered by that statement on the sheet, so specify the natural grade for a food-contact part and ask for the food contact declaration with the TDS and SDS.

How does Sipolprene 65215 compare with 68217?

Sipolprene 68217 is harder at Shore D 68 against 65, stiffer at 525 MPa against 470 MPa, and melts at 217 °C against 215 °C. Sipolprene 65215 holds no break in notched Izod at 23 °C where 68217 reads 37 J/m, and its abrasion loss is 55 mm³ against 56 mm³.

Can I get the TDS and SDS for Sipolprene 65215?

Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Sipolprene SP 215 LV

The same Shore D 65 property set at MFI 35, for easier mold filling.

Sipolprene 60212

Shore D 60 high-modulus grade at 460 MPa with 235 N/mm tear.

Sipolprene 68217

Harder at Shore D 68 and 525 MPa, with black and UV versions.

Where this grade fits

TPC-ET copolyester elastomers

The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.

What is TPC-ET

What the TPC-ET name means and how copolyester elastomer differs from TPU.

Matching a TPC-ET specification

Matching an existing specification by Shore D hardness, melt viscosity and version suffix.

Evaluating Sipolprene 65215?

Tell us the system you are formulating and the property you need to hit. We will confirm the grade, send the data sheet, and ship a sample.