TPC-ET at Shore D 72 with a 218 °C melting point and 660 MPa flexural modulus, with copper deactivation stabilization for jacketing cables that run hot.
Sipolprene 72220 is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 72, with a 218 °C melting point and a 660 MPa flexural modulus. Sipol's data sheet describes it with a copper deactivation stabilization package that suits it to jacketing cables working at high temperatures, and its melt flow of 19 g/10 min at 230 °C, 2.16 kg lets it be injection molded or extruded.
Sipol's description on that data sheet names the product 72220 MD. The sheet title and the safety data sheet name it 72220. When the order is for cable jacketing, say so on the request, so the copper deactivation package is confirmed for the material you receive.
The 218 °C melt and 210 °C Vicat A/50 give a jacket or part room to run hot, and the glass transition sits at 28 °C. Stress at break is 53 MPa and elongation at break 460 percent, and water absorption is 0.1 percent after 24 hours of immersion.
Notched Izod is 46 J/m at 23 °C and 36 J/m at -40 °C (ISO 180). Compression set is 18 percent at 23 °C and 70 percent at 70 °C, and abrasion loss is 76 mm³ (ISO 4649).
Two versions have their own Sipol data sheets. 72220 B is a black dry blend and 72220 W a UV-stabilized dry blend, both with the natural grade's typical values and processing profile. Their sheets do not mention the copper deactivation package.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 218 °C (ISO 11357-3) |
| Crystallization temperature | 183 °C (ISO 11357-3) |
| Glass transition temperature | 28 °C (ISO 11357-2) |
| Vicat softening temperature A/50 | 210 °C (ISO 306) |
| Melt flow index (MFI) | 19 g/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Melt volume rate (MVR) | 15 cm³/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 72 instantaneous, 69 after 15 s (ISO 868) |
| Stress at break | 53 MPa (ISO 527) |
| Elongation at break | 460 % (ISO 527) |
| Flexural modulus | 660 MPa (ISO 178) |
| Notched Izod impact at 23 °C | 46 J/m (ISO 180) |
| Notched Izod impact at -40 °C | 36 J/m (ISO 180) |
| Abrasion loss | 76 mm³ at 5 N vertical load (ISO 4649) |
| Compression set at 23 °C | 18 % (ISO 815:1991) |
| Compression set at 70 °C | 70 % (ISO 815:1991) |
| Density | 1.25 g/cm³ (ISO 1183) |
| Water absorption | 0.1 % after 24 h immersion at 23 °C (Sipol method MI 08) |
| Stabilization | Copper deactivation package (described on the 72220 sheet as 72220 MD) |
| Form | Granules |
| Versions | 72220 B (black dry blend), 72220 W (UV-stabilized dry blend) |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Sipol states the copper deactivation stabilization suits it to jacketing cables that work at high temperatures.
Sipol's profile runs 195 to 210 °C at the rear zone up to 240 °C at the nozzle, with the mold at 40 to 50 °C.
The extrusion profile climbs from 200 to 215 °C at the feed to 215 to 230 °C at the head and die.
72220 B is the black dry blend.
72220 W is the UV-stabilized dry blend.
Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.
For injection molding, Sipol suggests the rear zone at 195 to 210 °C, the center zone at 220 °C, the front zone at 230 °C and the nozzle at 240 °C, with the mold at 40 to 50 °C.
For extrusion, including cable jacketing, the suggested profile is feed zone 200 to 215 °C, compression zone 215 to 225 °C, metering zone 215 to 230 °C and head or die 215 to 230 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Read the safety data sheet before handling.
Sipol's data sheet describes Sipolprene 72220 as a Shore D 72 TPC-ET with a copper deactivation stabilization package that suits it to jacketing cables working at high temperatures. It melts at 218 °C with a 210 °C Vicat A/50 and a 660 MPa flexural modulus. At MFI 19 g/10 min it can also be injection molded or extruded into other parts.
Sipol's sheets for Sipolprene 72220 B and 72220 W do not say so. The black and UV-stabilized dry-blend sheets carry the same Shore D 72, 218 °C melt and 660 MPa flexural modulus as the natural grade, but only the natural grade's sheet describes the copper deactivation stabilization. For a black or UV-stabilized cable jacket, tell us the service temperature and we will confirm the stabilization with Sipol before you order.
Sipolprene 72220 melts at 218 °C. For injection molding Sipol suggests 195 to 210 °C at the rear zone, 220 °C center, 230 °C front and 240 °C at the nozzle, with the mold at 40 to 50 °C. For extrusion the profile runs 200 to 215 °C at the feed, 215 to 225 °C in compression, and 215 to 230 °C through metering and the die. Dry 2 to 3 hours at 90 °C first.
Sipol's data sheets for Sipolprene 72220, 72220 B and 72220 W carry no food contact statement, so we make no food contact claim for this grade. For a hard food-contact part, Sipolprene 68217 at Shore D 68 and 525 MPa flexural modulus is stated by Sipol to be in compliance with American FDA and European EU 10/2011 food contact regulations in its natural version.
Sipolprene 72220 is harder at Shore D 72 against 68 and stiffer at 660 MPa against 525 MPa, and its sheet describes the copper deactivation stabilization for hot cable jacketing. Sipolprene 68217 is stronger at break, 58 MPa against 53 MPa, wears less at 56 mm³ abrasion loss against 76 mm³, and carries a food contact statement.
Yes. We send the Technical Data Sheet (TDS) and Safety Data Sheet (SDS) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Shore D 68 at 525 MPa, with a food contact statement on the natural grade.
Shore D 65 at 470 MPa, no break in notched Izod at 23 °C.
Shore D 62 with an HV version at MFI 11 for extrusion.
The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.