Sipolprene 63210

TPC-ET at Shore D 62 with a 211 °C melting point, 320 MPa flexural modulus and MFI 23, plus an HV extrusion version at MFI 11. FDA and EU 10/2011.

Home › Products › Sipol › Sipolprene 63210

Sipolprene 63210 is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 62, with a 211 °C melting point and a melt flow of 23 g/10 min at 230 °C, 2.16 kg. Sipol designed it as a medium-modulus ether ester elastomer with a rheology suited to injection molding and extrusion.

The natural grade carries Sipol's standard stabilization package and, per Sipol's data sheet, is in compliance with American FDA and European EU 10/2011 food contact regulations.

Flexural modulus is 320 MPa, stress at break 48 MPa and elongation at break 470 percent. Notched Izod is 155 J/m at 23 °C and 82 J/m at -40 °C, against 80 J/m for Sipolprene 58210 and 20 J/m for 60212.

The 211 °C melt and 195 °C Vicat A/50 set the upper limit for heat exposure, and the glass transition sits at 3 °C. Compression set is 39 percent at 23 °C and 62 percent at 70 °C (ISO 815), and abrasion loss is 32 mm³ (ISO 4649).

Three versions have their own Sipol data sheets. 63210 B is a black dry blend and 63210 W a UV-stabilized dry blend, both with the natural grade's typical values. 63210 HV - IP 924 is the high-viscosity version at MFI 11 g/10 min, with its own hotter extrusion profile and the same FDA and EU 10/2011 statement; Sipol marks its sheet provisional.

It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.

Typical properties

PropertyTypical value
Melting temperature211 °C (ISO 11357-3)
Crystallization temperature167 °C (ISO 11357-3)
Glass transition temperature3 °C (ISO 11357-2)
Vicat softening temperature A/50195 °C (ISO 306)
Melt flow index (MFI)23 g/10 min at 230 °C, 2.16 kg (ISO 1133)
Melt volume rate (MVR)19 cm³/10 min at 230 °C, 2.16 kg (ISO 1133)
Shore D hardness62 instantaneous, 59 after 15 s (ISO 868)
Stress at break48 MPa (ISO 527)
Elongation at break470 % (ISO 527)
Flexural modulus320 MPa (ISO 178)
Notched Izod impact at 23 °C155 J/m (ISO 180)
Notched Izod impact at -40 °C82 J/m (ISO 180)
Abrasion loss32 mm³ at 5 N vertical load (ISO 4649)
Compression set at 23 °C39 % (ISO 815:1991)
Compression set at 70 °C62 % (ISO 815:1991)
Density1.22 g/cm³ (ISO 1183)
Water absorption0.2 % after 24 h immersion at 23 °C (Sipol method MI 08)
ColorNatural
FormGranules
Versions63210 B (black dry blend), 63210 W (UV-stabilized dry blend), 63210 HV - IP 924 (high viscosity, provisional sheet)
63210 HV - IP 924MFI 11 g/10 min at 230 °C, 2.16 kg (ISO 1133); Shore D, melting point, Tg, stress at break, elongation, flexural modulus, density and water absorption as the natural grade

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Injection molded parts

Sipol's profile runs 190 to 205 °C at the rear zone up to 235 °C at the nozzle, with the mold at 30 to 40 °C.

Extruded parts

The natural grade's extrusion profile climbs from 195 to 210 °C at the feed to 210 to 225 °C at the head and die.

High-viscosity extrusion

63210 HV - IP 924 runs at MFI 11 g/10 min with the die at 220 to 230 °C.

Food-contact parts

The natural grade and the HV - IP 924 version are stated in compliance with FDA and EU 10/2011 food contact regulations.

Black and UV-exposed parts

63210 B is the black dry blend and 63210 W the UV-stabilized dry blend.

Handling and dispersion

Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.

For injection molding the natural grade, Sipol suggests the rear zone at 190 to 205 °C, the center zone at 215 °C, the front zone at 225 °C and the nozzle at 235 °C, with the mold at 30 to 40 °C. For extrusion, the profile is feed zone 195 to 210 °C, compression zone 210 to 220 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C.

The 63210 HV - IP 924 version runs hotter. Its injection profile is rear zone 195 to 210 °C, center 220 °C, front 230 °C and nozzle 235 °C, and its extrusion profile is feed zone 200 to 215 °C, compression zone 215 to 225 °C, metering zone 220 to 230 °C and head or die 220 to 230 °C.

Packaging, storage, and regulatory status

Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..

Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.

Sipol states the natural grade and the HV - IP 924 version are in compliance with American FDA and European EU 10/2011 food contact regulations. Read the safety data sheet before handling.

Frequently asked questions

Which version of Sipolprene 63210 suits extrusion?

The natural grade at MFI 23 g/10 min (230 °C, 2.16 kg) is rated for extrusion. Sipolprene 63210 HV - IP 924 is the high-viscosity version at MFI 11 g/10 min, with the same Shore D 62 and 320 MPa flexural modulus. Its sheet calls for a hotter profile, 200 to 215 °C at the feed rising to 220 to 230 °C at the die, and Sipol marks it provisional.

Is Sipolprene 63210 suitable for hydraulic hose?

No, Sipolprene 63210 should not be used for hydraulic hose. Copolyester elastomers are not the material for hydraulic hose or oleodynamic service. Thermoplastic polyurethane is the material for hydraulic hose. The limit applies equally to the 63210 HV - IP 924 extrusion version at MFI 11 g/10 min.

What processing temperatures does Sipolprene 63210 need?

Sipolprene 63210 melts at 211 °C. For injection molding Sipol suggests 190 to 205 °C at the rear zone, 215 °C center, 225 °C front and 235 °C at the nozzle, with the mold at 30 to 40 °C. For extrusion the profile runs 195 to 210 °C at the feed, 210 to 220 °C in compression, and 210 to 225 °C through metering and the die. Dry first for 2 to 3 hours at 90 °C.

Is Sipolprene 63210 food-contact compliant?

Sipol's data sheet states that natural Sipolprene 63210 is in compliance with American FDA and European EU 10/2011 food contact regulations, and the 63210 HV - IP 924 sheet carries the same statement. The 63210 B and 63210 W dry-blend sheets do not, so a food-contact part should be specified in the natural grade or the HV version. Ask for the food contact declaration with the TDS and SDS.

What separates Sipolprene 63210 from Sipolprene 58210?

Sipolprene 63210 is Shore D 62 against 58 for 58210, with flexural modulus 320 MPa against 280 MPa and the same 211 °C melting point. Its Vicat A/50 is 195 °C against 190 °C. Cold impact is close, 82 J/m against 80 J/m notched Izod at -40 °C, and compression set at 23 °C is 39 percent against 20 percent.

Can I get the TDS and SDS for Sipolprene 63210?

Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Sipolprene 58210

Softer at Shore D 58, with an EK1 HV extrusion version at MFI 13.

Sipolprene 60212

Shore D 60 high-modulus grade at 460 MPa and 235 N/mm tear.

Sipolprene 68217

Stiffer at Shore D 68 and 525 MPa, with a 217 °C melt.

Where this grade fits

TPC-ET copolyester elastomers

The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.

What is TPC-ET

What the TPC-ET name means and how copolyester elastomer differs from TPU.

Matching a TPC-ET specification

Matching an existing specification by Shore D hardness, melt viscosity and version suffix.