TPC-ET at Shore D 58 with a 211 °C melting point, 280 MPa flexural modulus and MFI 23. Molding and extrusion, with an EK1 HV version at MFI 13.

Home › Products › Sipol › Sipolprene 58210

Sipolprene 58210 is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 58, with a 211 °C melting point and a melt flow of 23 g/10 min at 230 °C, 2.16 kg. Sipol designed it as a medium-modulus ether ester elastomer with a rheology suited to injection molding and extrusion.

The natural grade carries Sipol's standard stabilization package and, per Sipol's data sheet, is in compliance with American FDA and European EU 10/2011 food contact regulations.

Flexural modulus is 280 MPa, stress at break 44 MPa and elongation at break 530 percent. Notched Izod is 142 J/m at 23 °C and 80 J/m at -40 °C, with the glass transition at -8 °C, so a cold-service part should be tested at its lowest temperature.

Compression set is 20 percent at 23 °C and 67 percent at 70 °C (ISO 815). The 211 °C melt and 190 °C Vicat A/50 set the upper limit for heat exposure, and abrasion loss is 33 mm³ (ISO 4649).

Four versions have their own Sipol data sheets. 58210 B is a black dry blend, 58210 W a UV-stabilized dry blend and 58210 WB a UV-stabilized black dry blend, all with the natural grade's typical values. 58210 EK1 HV - IP 966 is a high-viscosity version at MFI 13 g/10 min, which Sipol lists as an experimental grade on a provisional sheet. That sheet carries the same FDA and EU 10/2011 statement as the natural grade.

It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.

Typical properties

PropertyTypical value
Melting temperature211 °C (ISO 11357-3)
Crystallization temperature174 °C (ISO 11357-3)
Glass transition temperature-8 °C (ISO 11357-2)
Vicat softening temperature A/50190 °C (ISO 306)
Melt flow index (MFI)23 g/10 min at 230 °C, 2.16 kg (ISO 1133)
Melt volume rate (MVR)19 cm³/10 min at 230 °C, 2.16 kg (ISO 1133)
Shore D hardness58 instantaneous, 55 after 15 s (ISO 868)
Stress at break44 MPa (ISO 527)
Elongation at break530 % (ISO 527)
Flexural modulus280 MPa (ISO 178)
Notched Izod impact at 23 °C142 J/m (ISO 180)
Notched Izod impact at -40 °C80 J/m (ISO 180)
Abrasion loss33 mm³ at 5 N vertical load (ISO 4649)
Compression set at 23 °C20 % (ISO 815:1991)
Compression set at 70 °C67 % (ISO 815:1991)
Density1.20 g/cm³ (ISO 1183)
Water absorption0.3 % after 24 h immersion at 23 °C (Sipol method MI 08)
ColorNatural
FormGranules
Versions58210 B (black dry blend), 58210 W (UV-stabilized dry blend), 58210 WB (UV-stabilized black dry blend), 58210 EK1 HV - IP 966 (high viscosity, experimental)
58210 EK1 HV - IP 966MFI 13 g/10 min and MVR 11 cm³/10 min at 230 °C, 2.16 kg (ISO 1133); crystallization 162 °C; stress at break 45 MPa; elongation 456 %; flexural modulus 241 MPa; Shore D, melting point, density and water absorption as the natural grade

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Injection molded parts

Sipol's profile runs 190 to 205 °C at the rear zone up to 235 °C at the nozzle, with the mold at 30 to 40 °C.

Extruded parts

The extrusion profile climbs from 195 to 210 °C at the feed to 210 to 225 °C at the head and die.

High-viscosity extrusion

58210 EK1 HV - IP 966 runs at MFI 13 g/10 min on the same extrusion profile.

Food-contact parts

The natural grade and the EK1 HV version are stated in compliance with FDA and EU 10/2011 food contact regulations.

Black and UV-exposed parts

58210 B is black, 58210 W UV-stabilized, and 58210 WB both, each as a dry blend.

Handling and dispersion

Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.

For injection molding, Sipol suggests the rear zone at 190 to 205 °C, the center zone at 215 °C, the front zone at 225 °C and the nozzle at 235 °C, with the mold at 30 to 40 °C. The W and WB sheets give 230 °C at the nozzle.

For extrusion, the suggested profile is feed zone 195 to 210 °C, compression zone 210 to 220 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C. The EK1 HV - IP 966 sheet gives the same injection and extrusion profiles.

Packaging, storage, and regulatory status

Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..

Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.

Sipol states the natural grade and the EK1 HV - IP 966 version are in compliance with American FDA and European EU 10/2011 food contact regulations. Read the safety data sheet before handling.

Frequently asked questions

What processing temperatures does Sipolprene 58210 need?

Sipolprene 58210 melts at 211 °C. For injection molding Sipol suggests 190 to 205 °C at the rear zone, 215 °C center, 225 °C front and 235 °C at the nozzle, with the mold at 30 to 40 °C. For extrusion the profile runs 195 to 210 °C at the feed, 210 to 220 °C in compression, and 210 to 225 °C through metering and the die. Dry first for 2 to 3 hours at 90 °C in a dehumidifying dryer.

Which version of Sipolprene 58210 suits extrusion?

The natural grade at MFI 23 g/10 min (230 °C, 2.16 kg) is rated for extrusion. Sipolprene 58210 EK1 HV - IP 966 is the high-viscosity version at MFI 13 g/10 min, with flexural modulus 241 MPa and elongation 456 percent. Sipol lists it as experimental on a provisional sheet dated 22/11/2024, so plan a trial before you write it into a specification.

Is Sipolprene 58210 food-contact compliant?

Sipol's data sheet states that natural Sipolprene 58210 is in compliance with American FDA and European EU 10/2011 food contact regulations, and the 58210 EK1 HV - IP 966 sheet carries the same statement. The B, W and WB dry-blend sheets do not, so a food-contact part should be specified in the natural grade or the EK1 HV version. Ask for the food contact declaration with the TDS and SDS.

How does Sipolprene 58210 sit between 54205 and 63210?

Sipolprene 58210 is Shore D 58, between 54205 at Shore D 54 and 63210 at Shore D 62. Flexural modulus steps from 200 MPa to 280 MPa to 320 MPa across the three, and melting point from 204 °C to 211 °C to 211 °C. Notched Izod at -40 °C reads no break for 54205, 80 J/m for 58210 and 82 J/m for 63210.

Can I get the TDS and SDS for Sipolprene 58210?

Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Sipolprene 54205

Softer at Shore D 54, no break in notched Izod at -40 °C.

Sipolprene 63210

Stiffer at Shore D 62 and 320 MPa, with an HV extrusion version at MFI 11.

Sipolprene 60212

Shore D 60 with a 460 MPa flexural modulus and 235 N/mm tear strength.

Where this grade fits

TPC-ET copolyester elastomers

The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.

What is TPC-ET

What the TPC-ET name means and how copolyester elastomer differs from TPU.

Matching a TPC-ET specification

Matching an existing specification by Shore D hardness, melt viscosity and version suffix.