Sipolprene 54205

TPC-ET at Shore D 54 with a 204 °C melting point, 22 percent compression set at 23 °C and MFI 20. Molding and extrusion, natural grade FDA and EU 10/2011.

Home › Products › Sipol › Sipolprene 54205

Sipolprene 54205 is a thermoplastic copolyester elastomer (TPC-ET) at Shore D 54, with a 204 °C melting point and a melt flow of 20 g/10 min at 230 °C, 2.16 kg. Sipol designed it as a medium-modulus ether ester elastomer with a rheology suited to injection molding and extrusion.

The natural grade carries Sipol's standard stabilization package and, per Sipol's data sheet, is in compliance with American FDA and European EU 10/2011 food contact regulations.

Compression set is 22 percent at 23 °C and 60 percent at 70 °C (ISO 815), and abrasion loss is 18 mm³ (ISO 4649). Those are the figures for a part that is squeezed or rubbed in service. Notched Izod is no break at 23 °C and at -40 °C, with the glass transition at -14 °C.

Flexural modulus is 200 MPa, stress at break 43 MPa and elongation at break 500 percent. The 204 °C melt and 182 °C Vicat A/50 set the upper limit for heat exposure.

Five versions have their own Sipol data sheets. 54205 B is a black dry blend, 54205 W a UV-stabilized dry blend and 54205 WB a UV-stabilized black dry blend, all carrying the natural grade's typical values. 54205 EK1 HV - IP 965 and 54205 E K2 HV - IP 964 are high-viscosity versions at MFI 14 g/10 min and Shore D 56, supplied natural with increased stabilization compared to the standard version. Sipol lists both as experimental grades on provisional sheets.

It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.

Typical properties

PropertyTypical value
Melting temperature204 °C (ISO 11357-3)
Crystallization temperature163 °C (ISO 11357-3)
Glass transition temperature-14 °C (ISO 11357-2)
Vicat softening temperature A/50182 °C (ISO 306)
Melt flow index (MFI)20 g/10 min at 230 °C, 2.16 kg (ISO 1133)
Melt volume rate (MVR)17 cm³/10 min at 230 °C, 2.16 kg (ISO 1133)
Shore D hardness54 instantaneous, 51 after 15 s (ISO 868)
Stress at break43 MPa (ISO 527)
Elongation at break500 % (ISO 527)
Flexural modulus200 MPa (ISO 178)
Notched Izod impact at 23 °CNo break (ISO 180)
Notched Izod impact at -40 °CNo break (ISO 180)
Abrasion loss18 mm³ at 5 N vertical load (ISO 4649)
Compression set at 23 °C22 % (ISO 815:1991)
Compression set at 70 °C60 % (ISO 815:1991)
Density1.21 g/cm³ (ISO 1183)
Water absorption0.30 % after 24 h immersion at 23 °C (Sipol method MI 08)
ColorNatural
FormGranules
Versions54205 B (black dry blend), 54205 W (UV-stabilized dry blend), 54205 WB (UV-stabilized black dry blend), 54205 EK1 HV - IP 965 and 54205 E K2 HV - IP 964 (high viscosity, increased stabilization, experimental)
54205 EK1 HV and E K2 HVMFI 14 g/10 min and MVR 12 cm³/10 min at 230 °C, 2.16 kg (ISO 1133); Shore D 56 instantaneous, 52 after 15 s; melting 205 °C; stress at break 48 MPa; elongation 522 %; flexural modulus 160 MPa; notched Izod no break at 23 °C and -40 °C

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Injection molded parts

Sipol's profile runs 185 to 200 °C at the rear zone up to 230 °C at the nozzle, with the mold at 30 to 40 °C.

Extruded parts

The extrusion profile climbs from 195 to 210 °C at the feed to 210 to 225 °C at the head and die.

High-viscosity extrusion

The EK1 HV and E K2 HV versions run at MFI 14 g/10 min on the same extrusion profile.

Food-contact parts

The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.

Black and UV-exposed parts

54205 B is black, 54205 W UV-stabilized, and 54205 WB both, each as a dry blend.

Handling and dispersion

Dry before processing. Sipol recommends 2 to 3 hours at 90 °C in a dehumidifying dryer and gives a processing moisture content of 0.15 percent.

For injection molding, Sipol suggests the rear zone at 185 to 200 °C, the center zone at 210 °C, the front zone at 220 °C and the nozzle at 230 °C, with the mold at 30 to 40 °C.

For extrusion, the suggested profile is feed zone 195 to 210 °C, compression zone 205 to 215 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C. The EK1 HV and E K2 HV sheets give the same injection and extrusion profiles.

Packaging, storage, and regulatory status

Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg or 1000 kg big bags..

Storage: Stable for 12 months unopened in the original packaging, kept in a cool, dry place and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.

Sipol states the natural grade is in compliance with American FDA and European EU 10/2011 food contact regulations. Read the safety data sheet before handling.

Frequently asked questions

What processing temperatures does Sipolprene 54205 need?

Sipolprene 54205 melts at 204 °C. For injection molding Sipol suggests 185 to 200 °C at the rear zone, 210 °C center, 220 °C front and 230 °C at the nozzle, with the mold at 30 to 40 °C. For extrusion the profile runs 195 to 210 °C at the feed, 205 to 215 °C in compression, and 210 to 225 °C through metering and the die. Dry first for 2 to 3 hours at 90 °C in a dehumidifying dryer.

Which version of Sipolprene 54205 suits extrusion?

The natural grade at MFI 20 g/10 min (230 °C, 2.16 kg) is rated for extrusion. Sipolprene 54205 EK1 HV - IP 965 and E K2 HV - IP 964 are the high-viscosity versions at MFI 14 g/10 min, Shore D 56, with increased stabilization over the standard version. Sipol lists both as experimental on provisional sheets, and the two sheets carry identical typical values, so tell us the service conditions and we will confirm which one Sipol recommends.

Is Sipolprene 54205 food-contact compliant?

Sipol's data sheet states that natural Sipolprene 54205 is in compliance with American FDA and European EU 10/2011 food contact regulations. The B, W and WB dry-blend sheets and the two HV sheets do not carry that statement, so a food-contact part should be specified in the natural grade. Ask for the food contact declaration with the TDS and SDS.

What separates Sipolprene 54205 from Sipolprene 55200?

Sipolprene 54205 is Shore D 54 against 53 for 55200, melts at 204 °C against 198 °C, and has a Vicat A/50 of 182 °C against 177 °C. Compression set at 23 °C is 22 percent against 42 percent, and abrasion loss is 18 mm³ against 24 mm³. Sipolprene 55200 stretches further, 590 percent elongation at break against 500.

Can I get the TDS and SDS for Sipolprene 54205?

Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Sipolprene 55200

Shore D 53 with a 198 °C melt and 590 percent elongation at break.

Sipolprene 55211

The same Shore D 54 with a 213 °C melt and MFI 12.

Sipolprene 58210

Stiffer at Shore D 58, with a 211 °C melt and an EK1 HV extrusion version.

Where this grade fits

TPC-ET copolyester elastomers

The Sipolprene range by hardness and melting point, and where copolyester elastomer does not fit.

What is TPC-ET

What the TPC-ET name means and how copolyester elastomer differs from TPU.

Matching a TPC-ET specification

Matching an existing specification by Shore D hardness, melt viscosity and version suffix.

Evaluating Sipolprene 54205?

Tell us the system you are formulating and the property you need to hit. We will confirm the grade, send the data sheet, and ship a sample.