Shore D 48 ether ester TPC-ET melting at 198 °C, with a 150 MPa flexural modulus and 0.4 percent water absorption. Natural grade meets FDA and EU 10/2011.
Sipolprene 48200 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 48, with a melting temperature of 198 °C and a low modulus. Sipol rates its melt behavior as suitable for injection molding and extrusion.
Flexural modulus is 150 MPa, stress at break 34 MPa and elongation at break 560 percent. The Vicat A softening point is 174 °C and the glass transition -18 °C, with no notched Izod break at 23 °C or -40 °C.
Compression set is 34 percent at 23 °C and 61 percent at 70 °C. Abrasion loss is 23 mm³ at 5 N, and water absorption is 0.4 percent after 24 hours of immersion.
Melt flow is 23 g/10 min at 230 °C and 2.16 kg. The suggested mold temperature is 30 to 40 °C, against 20 to 30 °C for Sipolprene 46185.
The natural grade comes with a standard stabilization package, and Sipol states it is in compliance with American FDA and European EU 10/2011 food contact regulations. Two dry blends have their own data sheets: 48200 B in black and 48200 W UV stabilized. Heat-stabilized dry blends are available on request.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 198 °C (ISO 11357-3) |
| Crystallization temperature | 152 °C (ISO 11357-3) |
| Glass transition temperature | -18 °C (ISO 11357-2) |
| Vicat softening, A/50 | 174 °C (ISO 306) |
| Melt flow index (MFI) | 23 g/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Melt volume rate (MVR) | 19 cm³/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 48 instantaneous, 46 after 15 s (ISO 868) |
| Stress at break | 34 MPa (ISO 527) |
| Elongation at break | 560 percent (ISO 527) |
| Flexural modulus | 150 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 23 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 34 percent (ISO 815:1991) |
| Compression set, 70 °C | 61 percent (ISO 815:1991) |
| Density | 1.18 g/cm³ (ISO 1183) |
| Water absorption | 0.4 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Color | Natural; black in the B dry blend |
| Versions | 48200 natural, 48200 B black, 48200 W UV stabilized; heat stabilized dry blend on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Shore D 48 with a 150 MPa flexural modulus, molded at 205 to 225 °C with the mold at 30 to 40 °C.
Extrusion profile of 190 to 205 °C at the feed and 210 to 225 °C at the die.
The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.
The 48200 W dry blend is UV stabilized.
Dry before processing at 90 °C for 2 to 3 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent.
Suggested injection molding profile for a 198 °C melting grade: rear zone 180 to 195 °C, center zone 205 °C, front zone 215 °C and nozzle 225 °C, with the mold at 30 to 40 °C.
Suggested extrusion profile: feeding zone 190 to 205 °C, compression zone 205 to 215 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Sipol states the natural grade, with its standard stabilization package, is in compliance with American FDA and European EU 10/2011 food contact regulations. The B and W dry blend data sheets carry no food contact statement. Read the safety data sheet before handling.
Sipolprene 48200 melts at 198 °C. Sipol suggests an injection barrel profile of 180 to 195 °C at the rear zone, 205 °C center, 215 °C front and 225 °C at the nozzle, with the mold at 30 to 40 °C. The extrusion profile runs 190 to 205 °C at the feed and 210 to 225 °C at the die. Dry 2 to 3 hours at 90 °C to 0.15 percent moisture first.
The natural Sipolprene 48200, with its standard stabilization package, is stated by Sipol to be in compliance with American FDA and European EU 10/2011 food contact regulations. It is a Shore D 48 grade melting at 198 °C. The 48200 B black and 48200 W UV-stabilized dry blends carry no food contact statement on their own data sheets.
Sipolprene 48200 is Shore D 48 against 45 for Sipolprene 46185, and it is close to twice as stiff, 150 MPa flexural modulus against 85 MPa. It melts higher, 198 °C against 186 °C, with a 174 °C Vicat point against 149 °C, and absorbs less water, 0.4 percent against 0.5. Both natural grades carry FDA and EU 10/2011 statements.
Sipolprene 48200 shows no break in notched Izod impact at -40 °C as well as at 23 °C, and its glass transition is -18 °C. Those are typical values on Sipol's data sheet at a nominal Shore D 48. A part that has to flex hard in the cold should be tested at its own service temperature.
Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Softer at Shore D 45 and 85 MPa, with the same FDA and EU 10/2011 statements.
Shore D 46 melting at 212 °C, with an HV version for extrusion.
The next step up in hardness, Shore D 54, melting at 204 °C.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means and how the family differs from TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.