Shore D 45 ether ester TPC-ET melting at 186 °C, with 33 MPa stress at break and 660 percent elongation. Natural grade meets FDA and EU 10/2011.
Sipolprene 46185 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 45, with a melting temperature of 186 °C and a low modulus. Sipol rates its melt behavior as suitable for injection molding and extrusion.
Stress at break is 33 MPa and elongation at break 660 percent, with a flexural modulus of 85 MPa. Notched Izod shows no break at 23 °C or -40 °C, and the glass transition is -38 °C.
Vicat A softening is 149 °C. Compression set is 34 percent at 23 °C and 69 percent at 70 °C, and abrasion loss is 24 mm³ at 5 N.
Water absorption is 0.5 percent after 24 hours of immersion, and the grade dries in 2 to 3 hours at 90 °C. Melt flow is 34 g/10 min at 230 °C and 2.16 kg.
The natural grade comes with a standard stabilization package, and Sipol states it is in compliance with American FDA and European EU 10/2011 food contact regulations. Two dry blends have their own data sheets with the same property table: 46185 B in black and 46185 W UV stabilized. Heat-stabilized dry blends are available on request.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 186 °C (ISO 11357-3) |
| Crystallization temperature | 131 °C (ISO 11357-3) |
| Glass transition temperature | -38 °C (ISO 11357-2) |
| Vicat softening, A/50 | 149 °C (ISO 306) |
| Melt flow index (MFI) | 34 g/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Melt volume rate (MVR) | 30 cm³/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 45 instantaneous, 42 after 15 s (ISO 868) |
| Stress at break | 33 MPa (ISO 527) |
| Elongation at break | 660 percent (ISO 527) |
| Flexural modulus | 85 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 24 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 34 percent (ISO 815:1991) |
| Compression set, 70 °C | 69 percent (ISO 815:1991) |
| Density | 1.15 g/cm³ (ISO 1183) |
| Water absorption | 0.5 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Color | Natural; black in the B dry blend |
| Versions | 46185 natural, 46185 B black, 46185 W UV stabilized; heat stabilized dry blend on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Extrusion profile of 175 to 190 °C at the feed and 190 to 205 °C at the die.
Shore D 45 with an 85 MPa flexural modulus, molded at 190 to 210 °C barrel temperatures.
The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.
The 46185 W dry blend is UV stabilized.
Dry before processing at 90 °C for 2 to 3 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent.
Suggested injection molding profile for a 186 °C melting grade: rear zone 165 to 180 °C, center zone 190 °C, front zone 200 °C and nozzle 210 °C, with the mold at 20 to 30 °C.
Suggested extrusion profile: feeding zone 175 to 190 °C, compression zone 185 to 195 °C, metering zone 190 to 205 °C and head or die 190 to 205 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Sipol states the natural grade, with its standard stabilization package, is in compliance with American FDA and European EU 10/2011 food contact regulations. The B and W dry blend data sheets carry no food contact statement. Read the safety data sheet before handling.
The natural Sipolprene 46185, with its standard stabilization package, is stated by Sipol to be in compliance with American FDA and European EU 10/2011 food contact regulations. It is a Shore D 45 grade melting at 186 °C. The 46185 B black and 46185 W UV-stabilized dry blends carry no food contact statement on their own data sheets, so specify the natural grade for food contact.
Sipolprene 46185 melts at 186 °C. Sipol suggests an injection barrel profile of 165 to 180 °C at the rear zone, 190 °C center, 200 °C front and 210 °C at the nozzle, with the mold at 20 to 30 °C. The extrusion profile runs 175 to 190 °C at the feed and 190 to 205 °C at the die. Dry 2 to 3 hours at 90 °C to 0.15 percent moisture.
Both are nominal Shore D 45. Sipolprene 46185 melts at 186 °C with 149 °C Vicat; Sipolprene 45211 melts at 209 °C with 186 °C Vicat. 46185 is stiffer at 85 MPa flexural modulus, stronger at 33 MPa stress at break against 23 MPa, stretches to 660 percent against 390, absorbs 0.5 percent water against 3.5, and carries FDA and EU 10/2011 statements.
Sipolprene 48200 is the next step up, Shore D 48 against 45, melting at 198 °C against 186 °C. It is much stiffer at 150 MPa flexural modulus against 85 MPa, with a 174 °C Vicat point against 149 °C. Both natural grades carry FDA and EU 10/2011 statements and both have B and W dry blends.
Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Same Shore D 45, melting at 209 °C with a 186 °C Vicat point.
Shore D 48 and stiffer at 150 MPa, also with FDA and EU 10/2011 statements.
Softer at Shore D 36, melting at 195 °C, with the same food contact statements.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means and how the family differs from TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.