Shore D 46 ether ester TPC-ET melting at 212 °C, high flow at 60 g/10 min, with a 25 g/10 min HV version for extrusion. Injection molding and extrusion.
Sipolprene 44210 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 46, with a melting temperature of 212 °C. Sipol rates its melt behavior as suitable for injection molding and extrusion.
The standard grade is high flow, at 60 g/10 min measured at 230 °C and 2.16 kg, which suits filling long or thin sections in a mold. Sipolprene 44210 HV is the high viscosity version on its own data sheet, at 25 g/10 min, with the same hardness, melting point and mechanical table.
Stress at break is 30 MPa, elongation at break 550 percent and flexural modulus 45 MPa. Abrasion loss is 22 mm³ at 5 N, and notched Izod shows no break at 23 °C or -40 °C.
Compression set is 30 percent at 23 °C and 53 percent at 70 °C, a smaller rise with temperature than Sipolprene 45211, 46185 or 48200 show. The crystallization temperature is 157 °C.
Black, UV-stabilized and heat-stabilized dry blends are available on request. The data sheet carries no food contact statement.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 212 °C (ISO 11357-3) |
| Crystallization temperature | 157 °C (ISO 11357-3) |
| Melt flow index (MFI) | 60 g/10 min at 230 °C, 2.16 kg (ISO 1133); 25 g/10 min for 44210 HV |
| Melt volume rate (MVR) | 51 cm³/10 min at 230 °C, 2.16 kg (ISO 1133); 21 for 44210 HV |
| Shore D hardness | 46 instantaneous, 43 after 15 s (ISO 868) |
| Stress at break | 30 MPa (ISO 527) |
| Elongation at break | 550 percent (ISO 527) |
| Flexural modulus | 45 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 22 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 30 percent (ISO 815:1991) |
| Compression set, 70 °C | 53 percent (ISO 815:1991) |
| Density | 1.18 g/cm³ (ISO 1183) |
| Water absorption | 0.7 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Versions | 44210 standard, 44210 HV high viscosity; black, UV and heat stabilized dry blends on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
The standard grade at 60 g/10 min, molded at 210 to 225 °C barrel temperatures.
44210 HV at 25 g/10 min, with an extrusion profile of 195 to 210 °C at the feed and 210 to 225 °C at the die.
Sipol supplies black, UV-stabilized and heat-stabilized dry blends of 44210 on request.
Dry before processing at 90 °C for 3 to 4 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent.
Suggested injection molding profile for a 212 °C melting grade: rear zone 200 °C, center zone 210 °C, front zone 220 °C and nozzle 225 °C, with the mold at 20 to 30 °C.
Suggested extrusion profile, the same on the standard and HV data sheets: feeding zone 195 to 210 °C, compression zone 205 to 215 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Read the safety data sheet before handling. The data sheet carries no food contact statement.
Sipolprene 44210 HV is the high viscosity version at 25 g/10 min melt flow, against 60 g/10 min for the standard grade, both at 230 °C and 2.16 kg. Shore D 46, the 212 °C melting point and the mechanical table are the same. The extrusion profile on both data sheets runs 195 to 210 °C at the feed and 210 to 225 °C at the die. The standard grade's high flow suits injection molding.
No. Sipolprene 44210 HV is a Shore D 46 copolyester elastomer, and TPC-ET is not the material for hydraulic hose or oleodynamic service. Thermoplastic polyurethane is the family for hydraulic hose. The HV version is for extrusion, where 25 g/10 min melt flow at 230 °C holds the melt in the die better than the standard 60 g/10 min.
The two sit a point apart in hardness, Shore D 46 for Sipolprene 44210 and 45 for Sipolprene 46185. 44210 melts higher, 212 °C against 186 °C, and flows faster, 60 g/10 min against 34. 46185 is stiffer at 85 MPa flexural modulus against 45 MPa and carries FDA and EU 10/2011 statements that the 44210 data sheet does not.
Sipolprene 44210 calls for 3 to 4 hours at 90 °C in a dehumidifying dryer, to a processing moisture content of 0.15 percent. Water absorption is 0.7 percent after 24 hours of immersion at 23 °C. The same drying conditions are on the 44210 HV data sheet. Sipol packs both in 25 kg bags with an aluminum film barrier against moisture, as well as octabins with a PE liner and big bags.
Yes. We send the Technical Data Sheet (TDS) and Safety Data Sheet (SDS) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Shore D 45, stiffer, with FDA and EU 10/2011 statements.
Shore D 45 melting at 209 °C, at a lower 16 g/10 min melt flow.
Shore D 48 with a 150 MPa flexural modulus and food contact statements.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means, how the family differs from TPU, and why hydraulics belong to TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.