Shore D 45 ether ester TPC-ET melting at 209 °C, with a 186 °C Vicat softening point and 169 °C crystallization. Injection molding and extrusion.
Sipolprene 45211 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 45, with a melting temperature of 209 °C and a medium modulus. Sipol rates its melt behavior as suitable for injection molding and extrusion.
Its Vicat A softening point is 186 °C, 23 °C under the melting point. The glass transition sits at -7 °C, and notched Izod still shows no break at 23 °C or at -40 °C.
Crystallization temperature is 169 °C, against 131 °C for Sipolprene 46185 at the same hardness. Flexural modulus is 75 MPa, stress at break 23 MPa and elongation at break 390 percent.
Compression set is 28 percent at 23 °C and 64 percent at 70 °C. Abrasion loss is 22 mm³ at 5 N. Water absorption is 3.5 percent after 24 hours of immersion, and the data sheet calls for 3 to 4 hours of drying.
Two dry blends have their own data sheets with the same property table: 45211 B in black and 45211 W UV stabilized. Heat-stabilized dry blends are available on request. No 45211 data sheet carries a food contact statement.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 209 °C (ISO 11357-3) |
| Crystallization temperature | 169 °C (ISO 11357-3) |
| Glass transition temperature | -7 °C (ISO 11357-2) |
| Vicat softening, A/50 | 186 °C (ISO 306) |
| Melt flow index (MFI) | 16 g/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Melt volume rate (MVR) | 14 cm³/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 45 instantaneous, 42 after 15 s (ISO 868) |
| Stress at break | 23 MPa (ISO 527) |
| Elongation at break | 390 percent (ISO 527) |
| Flexural modulus | 75 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 22 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 28 percent (ISO 815:1991) |
| Compression set, 70 °C | 64 percent (ISO 815:1991) |
| Density | 1.17 g/cm³ (ISO 1183) |
| Water absorption | 3.5 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Color | Black in the B dry blend |
| Versions | 45211 standard, 45211 B black, 45211 W UV stabilized; heat stabilized dry blend on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Shore D 45 with a 75 MPa flexural modulus, molded at 215 to 235 °C barrel temperatures.
Extrusion profile of 195 to 210 °C at the feed and 210 to 225 °C at the die.
A 186 °C Vicat softening point on a Shore D 45 elastomer.
The 45211 W dry blend is UV stabilized.
Dry before processing at 90 °C for 3 to 4 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent. The grade absorbs 3.5 percent water in 24 hours of immersion, so keep to the full drying time.
Suggested injection molding profile for a 209 °C melting grade: rear zone 190 to 205 °C, center zone 215 °C, front zone 225 °C and nozzle 235 °C, with the mold at 20 to 30 °C.
Suggested extrusion profile: feeding zone 195 to 210 °C, compression zone 205 to 215 °C, metering zone 210 to 225 °C and head or die 210 to 225 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Read the safety data sheet before handling. The 45211 data sheets carry no food contact statement.
Sipolprene 45211 has a Vicat A softening point of 186 °C against a melting temperature of 209 °C, at a nominal Shore D 45. Those are typical values from Sipol's data sheet and not a continuous service rating, so a part that runs hot for long periods should be qualified at temperature. Compression set at 70 °C is 64 percent.
Sipolprene 45211 melts at 209 °C. Sipol suggests an injection barrel profile of 190 to 205 °C at the rear zone, 215 °C center, 225 °C front and 235 °C at the nozzle, with the mold at 20 to 30 °C. The extrusion profile runs 195 to 210 °C at the feed and 210 to 225 °C at the die. Dry 3 to 4 hours at 90 °C first.
Both are Shore D 45. Sipolprene 45211 melts at 209 °C with a 186 °C Vicat point; Sipolprene 46185 melts at 186 °C with 149 °C Vicat. 46185 is stiffer at 85 MPa against 75 MPa, stretches further, 660 percent against 390, flows faster at 34 g/10 min against 16, absorbs 0.5 percent water against 3.5, and carries FDA and EU 10/2011 statements that 45211 does not.
The Sipolprene 45211 data sheets, natural, B and W, carry no food contact statement, so we do not describe the grade as compliant. At the same Shore D 45, Sipolprene 46185 is the grade whose natural version Sipol states is in compliance with American FDA and European EU 10/2011 food contact regulations, at a 186 °C melting point.
Yes. We send the Technical Data Sheet (TDS) and Safety Data Sheet (SDS) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Same Shore D 45, melting at 186 °C, with FDA and EU 10/2011 statements.
Shore D 46 melting at 212 °C, high flow at 60 g/10 min, with an HV version.
Softer at Shore D 38 and 170 °C, with an EU 10/2011 statement.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means and how the family differs from TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.