Shore D 36 ether ester TPC-ET melting at 195 °C, with 137 °C Vicat softening and 22 percent compression set at 23 °C. Natural grade meets FDA and EU 10/2011.
Sipolprene 35195 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 36, with a melting temperature of 195 °C and a low modulus. Sipol rates its melt behavior as suitable for injection molding and extrusion.
The 195 °C melting point and 137 °C Vicat A softening point give a soft part more heat headroom than Sipolprene 35180 at nearly the same hardness. Flexural modulus is 50 MPa, elongation at break 700 percent and stress at break 21 MPa.
Compression set is 22 percent at 23 °C and 63 percent at 70 °C. Abrasion loss is 27 mm³ at 5 N, and notched Izod shows no break at 23 °C or -40 °C, with a glass transition of -45 °C.
Melt flow is 28 g/10 min at 230 °C and 2.16 kg, and the processing profiles run hotter than the Shore D 35 grade, up to 220 °C at the nozzle and the die.
The natural grade comes with a standard stabilization package, and Sipol states it is in compliance with American FDA and European EU 10/2011 food contact regulations. Three dry blends have their own data sheets with the same property table: 35195 B in black, 35195 W UV stabilized, and 35195 WB UV stabilized in black. Heat-stabilized dry blends are available on request.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 195 °C (ISO 11357-3) |
| Crystallization temperature | 131 °C (ISO 11357-3) |
| Glass transition temperature | -45 °C (ISO 11357-2) |
| Vicat softening, A/50 | 137 °C (ISO 306) |
| Melt flow index (MFI) | 28 g/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Melt volume rate (MVR) | 25 cm³/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 36 instantaneous, 33 after 15 s (ISO 868) |
| Stress at break | 21 MPa (ISO 527) |
| Elongation at break | 700 percent (ISO 527) |
| Flexural modulus | 50 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 27 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 22 percent (ISO 815:1991) |
| Compression set, 70 °C | 63 percent (ISO 815:1991) |
| Density | 1.11 g/cm³ (ISO 1183) |
| Water absorption | 0.7 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Color | Natural; black in the B and WB dry blends |
| Versions | 35195 natural, 35195 B black, 35195 W UV stabilized, 35195 WB UV stabilized black; heat stabilized dry blend on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Shore D 36 with a 137 °C Vicat point, molded at 200 to 220 °C barrel temperatures.
Extrusion profile of 185 to 200 °C at the feed and 205 to 220 °C at the die.
The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.
The 35195 W and 35195 WB dry blends are UV stabilized.
Dry before processing at 90 °C for 2 to 3 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent.
Suggested injection molding profile for a 195 °C melting grade: rear zone 175 to 190 °C, center zone 200 °C, front zone 210 °C and nozzle 220 °C, with the mold at 20 to 30 °C.
Suggested extrusion profile: feeding zone 185 to 200 °C, compression zone 195 to 205 °C, metering zone 205 to 220 °C and head or die 205 to 220 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Sipol states the natural grade, with its standard stabilization package, is in compliance with American FDA and European EU 10/2011 food contact regulations. The B, W and WB dry blend data sheets carry no food contact statement. Read the safety data sheet before handling.
Sipolprene 35195 pairs a nominal Shore D 36 with a 195 °C melting point and a 137 °C Vicat A softening point. That melting point is above Sipolprene 35180 at 177 °C and Sipolprene 25185 at 184 °C, so it is the soft grade to look at when the part sees heat in service or in a downstream step. Compression set at 23 °C is 22 percent.
Sipolprene 35195 melts at 195 °C. Sipol suggests an injection barrel profile of 175 to 190 °C at the rear zone, 200 °C center, 210 °C front and 220 °C at the nozzle, with the mold at 20 to 30 °C. The extrusion profile runs 185 to 200 °C at the feed and 205 to 220 °C at the die. Dry at 90 °C for 2 to 3 hours to 0.15 percent moisture first.
The natural Sipolprene 35195, with its standard stabilization package, is stated by Sipol to be in compliance with American FDA and European EU 10/2011 food contact regulations. The 35195 B, 35195 W and 35195 WB dry blends carry no food contact statement on their own data sheets, so specify the natural grade where food contact applies.
Sipolprene 35195 melts at 195 °C with 137 °C Vicat; Sipolprene 35180 melts at 177 °C with 111 °C Vicat, at nearly the same hardness. 35180 is stiffer and stronger, 60 MPa flexural modulus and 28 MPa stress at break against 50 MPa and 21 MPa, and has an HV version at 19 g/10 min. 35195 has the lower compression set, 22 percent at 23 °C against 25 percent.
Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Shore D 35 melting at 177 °C, stiffer, with an HV version for extrusion.
Shore D 45 with an 85 MPa flexural modulus and the same FDA and EU 10/2011 statements.
Softer at Shore D 29, melting at 184 °C.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means and how the family differs from TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.