Shore D 35 ether ester TPC-ET melting at 177 °C, 34 g/10 min melt flow, with a 19 g/10 min HV version. Natural and HV grades meet FDA and EU 10/2011.
Sipolprene 35180 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 35, with a melting temperature of 177 °C and a low modulus. Sipol rates its melt behavior as suitable for injection molding and extrusion.
Flexural modulus is 60 MPa, stress at break 28 MPa and elongation at break 630 percent. Abrasion loss is 26 mm³ at 5 N, and notched Izod shows no break at 23 °C or -40 °C, with a glass transition of -46 °C.
Vicat A softening is 111 °C. Compression set is 25 percent at 23 °C and 68 percent at 70 °C.
The standard grade flows at 34 g/10 min at 230 °C and 2.16 kg. Sipolprene 35180 HV carries the same hardness, melting point and mechanical table at 19 g/10 min, and the lower melt flow is the version to ask about where the melt has to hold its shape out of a die.
The natural grade and 35180 HV come with a standard stabilization package, and Sipol states both are in compliance with American FDA and European EU 10/2011 food contact regulations. Three dry blends have their own data sheets: 35180 B in black, 35180 W UV stabilized, and 35180 WB UV stabilized in black. Heat-stabilized dry blends are available on request.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 177 °C (ISO 11357-3) |
| Crystallization temperature | 116 °C (ISO 11357-3) |
| Glass transition temperature | -46 °C (ISO 11357-2) |
| Vicat softening, A/50 | 111 °C (ISO 306) |
| Melt flow index (MFI) | 34 g/10 min at 230 °C, 2.16 kg (ISO 1133); 19 g/10 min for 35180 HV |
| Melt volume rate (MVR) | 31 cm³/10 min at 230 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 35 instantaneous, 33 after 15 s (ISO 868) |
| Stress at break | 28 MPa (ISO 527) |
| Elongation at break | 630 percent (ISO 527) |
| Flexural modulus | 60 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 26 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 25 percent (ISO 815:1991) |
| Compression set, 70 °C | 68 percent (ISO 815:1991) |
| Density | 1.11 g/cm³ (ISO 1183) |
| Water absorption | 0.70 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Color | Natural; black in the B and WB dry blends |
| Versions | 35180 natural, 35180 HV high viscosity, 35180 B black, 35180 W UV stabilized, 35180 WB UV stabilized black; heat stabilized dry blend on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Extrusion profile of 165 to 180 °C at the feed and 180 to 195 °C at the die, with the HV version at 19 g/10 min.
Shore D 35 with a 60 MPa flexural modulus, molded at 185 to 205 °C barrel temperatures.
The natural grade and 35180 HV are stated in compliance with FDA and EU 10/2011 food contact regulations.
The 35180 W and 35180 WB dry blends are UV stabilized.
Dry before processing at 90 °C for 2 to 3 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent.
Suggested injection molding profile for a 177 °C melting grade: rear zone 160 to 175 °C, center zone 185 °C, front zone 195 °C and nozzle 205 °C, with the mold at 20 to 30 °C.
Suggested extrusion profile, the same on the standard and HV data sheets: feeding zone 165 to 180 °C, compression zone 175 to 185 °C, metering zone 180 to 195 °C and head or die 180 to 195 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Sipol states the natural grade and 35180 HV, each with a standard stabilization package, are in compliance with American FDA and European EU 10/2011 food contact regulations. The B, W and WB dry blend data sheets carry no food contact statement. Read the safety data sheet before handling.
Sipolprene 35180 HV is the high viscosity version, at 19 g/10 min melt flow against 34 g/10 min for the standard grade, both measured at 230 °C and 2.16 kg. Hardness, the 177 °C melting point and the mechanical table are unchanged, and the extrusion temperature profile on both data sheets runs 165 to 180 °C at the feed and 180 to 195 °C at the die.
No. Sipolprene 35180 HV is a Shore D 35 copolyester elastomer, and TPC-ET is not the material for hydraulic hose or oleodynamic service. Thermoplastic polyurethane is the family for that job. The HV version is for extrusion where a melt flow of 19 g/10 min at 230 °C suits the die better than the standard 34 g/10 min.
The natural Sipolprene 35180 and Sipolprene 35180 HV, each with a standard stabilization package, are stated by Sipol to be in compliance with American FDA and European EU 10/2011 food contact regulations. The 35180 B, W and WB dry blends carry no food contact statement on their own data sheets, so specify the natural or HV grade where food contact applies.
Sipolprene 35180 melts at 177 °C with a 111 °C Vicat point; Sipolprene 35195 melts at 195 °C with 137 °C Vicat, at nearly the same hardness, Shore D 36 against 35. 35180 is stiffer at 60 MPa flexural modulus against 50 MPa and stronger at 28 MPa against 21 MPa stress at break, and it has an HV version that 35195 does not.
Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Shore D 36 melting at 195 °C, for parts that need more heat headroom.
Shore D 37 melting at 150 °C, developed for plasticizer-free PVC blends.
Shore D 45 at a similar 186 °C melting point, with the same FDA and EU 10/2011 statements.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means, how the family differs from TPU, and why hydraulics belong to TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.