Shore D 28 ether ester TPC-ET melting at 173 °C, with a -65 °C glass transition and no notched Izod break at -40 °C. Natural grade meets FDA and EU 10/2011.
Sipolprene 25170 is an ether ester thermoplastic elastomer (TPC-ET) at a nominal Shore D 28, with a melting temperature of 173 °C. Sipol rates its melt behavior as suitable for both injection molding and extrusion.
It is one of the softest grades in the range, with a flexural modulus of 25 MPa and elongation at break of 830 percent. Stress at break is 23 MPa.
The glass transition sits at -65 °C, and notched Izod shows no break at 23 °C or at -40 °C, so the part stays flexible well below freezing. Vicat A softening is 73 °C, which is the figure to check against the warm end of the service range.
Compression set is 26 percent at 23 °C and 67 percent at 70 °C. Melt flow is 12 g/10 min at 200 °C and 2.16 kg.
The natural grade comes with a standard stabilization package and Sipol states it is in compliance with American FDA and European EU 10/2011 food contact regulations. Three dry blend versions have their own data sheets with the same property table: 25170 B in black, 25170 W UV stabilized, and 25170 WB UV stabilized in black. Sipol also offers a heat-stabilized dry blend on request.
It is also written as TPC-ET, thermoplastic copolyester elastomer, TPEE, TEEE, COPE, copolyester elastomer, thermoplastic polyester elastomer, and ether ester elastomer.
| Property | Typical value |
|---|---|
| Melting temperature | 173 °C (ISO 11357-3) |
| Crystallization temperature | 105 °C (ISO 11357-3) |
| Glass transition temperature | -65 °C (ISO 11357-2) |
| Vicat softening, A/50 | 73 °C (ISO 306) |
| Melt flow index (MFI) | 12 g/10 min at 200 °C, 2.16 kg (ISO 1133) |
| Melt volume rate (MVR) | 11 cm³/10 min at 200 °C, 2.16 kg (ISO 1133) |
| Shore D hardness | 28 instantaneous, 25 after 15 s (ISO 868) |
| Stress at break | 23 MPa (ISO 527) |
| Elongation at break | 830 percent (ISO 527) |
| Flexural modulus | 25 MPa (ISO 178) |
| Notched Izod impact, 23 °C | No break (ISO 180) |
| Notched Izod impact, -40 °C | No break (ISO 180) |
| Abrasion resistance | 45 mm³ at 5 N vertical load (ISO 4649) |
| Compression set, 23 °C | 26 percent (ISO 815:1991) |
| Compression set, 70 °C | 67 percent (ISO 815:1991) |
| Density | 1.09 g/cm³ (ISO 1183) |
| Water absorption | 0.8 percent, 24 h immersion at 23 °C (Sipol method MI 08) |
| Color | Natural; black in the B and WB dry blends |
| Versions | 25170 natural, 25170 B black, 25170 W UV stabilized, 25170 WB UV stabilized black; heat stabilized dry blend on request |
Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.
Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.
Shore D 28 and a 25 MPa flexural modulus, molded at 180 to 200 °C barrel temperatures.
Extrusion profile of 160 to 180 °C at the feed and 180 to 195 °C at the die.
The natural grade is stated in compliance with FDA and EU 10/2011 food contact regulations.
The 25170 W and 25170 WB dry blends are UV stabilized.
Dry before processing at 90 °C for 2 to 3 hours in a dehumidifying dryer, to a processing moisture content of 0.15 percent.
Suggested injection molding profile for a 173 °C melting grade: rear zone 155 to 170 °C, center zone 180 °C, front zone 190 °C and nozzle 200 °C, with the mold at 20 to 30 °C.
Suggested extrusion profile: feeding zone 160 to 180 °C, compression zone 175 to 185 °C, metering zone 180 to 195 °C and head or die 180 to 195 °C.
Package sizes: 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..
Storage: Stable for 12 months unopened in the original packaging, kept cool and dry and protected from light. Material held at around 5 to 10 °C or below should sit at 15 to 20 °C for at least 24 hours before use.
Sipol states the natural grade, with its standard stabilization package, is in compliance with American FDA and European EU 10/2011 food contact regulations. The B, W and WB dry blend data sheets carry no food contact statement. Read the safety data sheet before handling.
The natural Sipolprene 25170, at Shore D 28 with its standard stabilization package, is stated by Sipol to be in compliance with American FDA and European EU 10/2011 food contact regulations. That statement sits on the natural grade's data sheet only. The 25170 B, W and WB dry blends carry no food contact statement on their own sheets, so specify the natural grade where food contact applies.
Sipolprene 25170 W is the UV-stabilized dry blend and 25170 WB is UV stabilized in black. Both have their own data sheets with the same Shore D 28, 173 °C melting point and 12 g/10 min melt flow as the natural grade. 25170 B is black without the UV statement. A heat-stabilized dry blend is available on request.
Sipolprene 25170 has a glass transition temperature of -65 °C, and notched Izod impact shows no break at both 23 °C and -40 °C. Flexural modulus at room temperature is 25 MPa. Those figures put it among the grades to look at for soft parts that have to flex in freezing conditions.
Sipolprene 25170 is Shore D 28 with a 173 °C melting point and 73 °C Vicat. Sipolprene 25185 is a point harder at Shore D 29, melts at 184 °C and softens at 98 °C Vicat, with a 35 MPa flexural modulus against 25 MPa. Choose 25185 where the part runs warmer, and 25170 for the softest response and 830 percent elongation.
Yes. We send the Technical Data Sheet (TDS), Safety Data Sheet (SDS), and Food contact declaration (FDA, EU 10/2011) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.
Shore D 29 with a higher 184 °C melting point and 98 °C Vicat.
Shore D 24, melting at 150 °C, developed for plasticizer-free PVC blends.
The next step up in hardness at Shore D 35, with an HV version.
The Sipolprene range from soft to hard, and where copolyester elastomer fits against TPU.
What the TPC-ET name means and how the family differs from TPU.
How to match a copolyester elastomer specification by hardness, melt flow and version.