Technipol PA 162

Copolyamide rod cement for automatic lasting machines, including toe lasters with tracers. 188 °C softening point, 8.0 Pa·s at 232 °C, rod of 3.9 or 4.2 mm.

Home › Products › Sipol › Technipol PA 162

Technipol PA 162 is an amber copolyamide hot melt extruded into rod, with a softening point of 188 °C and a Brookfield viscosity of 8.0 Pa·s at 232 °C. Sipol makes it for automatic lasting machines in the footwear industry, and designed it to run on toe lasting machines equipped with tracers as well.

Sipol credits it with a quick setting time, good flexibility, excellent wettability and high adhesion to leather and to both synthetic and regenerated materials. Footwear constructions vary widely, and Sipol recommends preliminary trials to approve the grade on the actual materials.

The 188 °C softening point and 8.0 Pa·s viscosity make PA 162 the higher-softening, heavier-bodied of Sipol's two copolyamide lasting rods. Technipol PA 167 softens at 172 °C and measures 3.5 Pa·s at the same 232 °C. The PA 162-4.2 data sheet gives an indicative application temperature of 220 to 240 °C.

Three versions exist. PA 162 is rod of 3.9 mm, PA 162-4.2 is rod of 4.2 mm for machines that take the larger diameter, and PA 162/G is the same polymer in granules, mainly used as raw material for extruding the rod. All three state more than 80 percent raw materials from non-edible renewable resources.

It is also written as copolyamide hot melt adhesive, co-polyamide hot melt, polyamide hot melt adhesive, polyamide rod cement, thermoplastic polyamide adhesive, and CoPA.

Typical properties

PropertyTypical value
Softening point188 °C (Sipol method MI 13)
Brookfield viscosity8.0 Pa·s at 232 °C (Sipol method MI 12, Brookfield CAP 2000+ cone and plate)
Density0.98 g/cm³ (ISO 1183)
Rod diameter3.9 ± 0.1 mm (PA 162), 4.2 ± 0.1 mm (PA 162-4.2)
Indicative application temperature220 to 240 °C (PA 162-4.2 data sheet)
Renewable raw materialsMore than 80 percent, from non-edible renewable resources (Sipol data sheet)
ColorAmber
FormRod on reels (PA 162, PA 162-4.2), granules (PA 162/G)
VersionsPA 162 (3.9 mm rod), PA 162-4.2 (4.2 mm rod), PA 162/G (granules for rod extrusion)

Typical values from the manufacturer's technical data sheet. They describe the product, they are not a specification. We will send the current TDS and the batch documentation your qualification needs.

Need this in your system?

Tell us the part or the process, the property you are targeting, and the volume you expect. We will confirm the grade, send the documentation, and get a sample of the candidate grade to you.

Applications

Automatic lasting machines

The rod cement Sipol makes PA 162 for.

Toe lasting with tracers

Sipol designed PA 162 to run on toe lasting machines equipped with tracers.

Leather

Sipol lists high adhesion to leather.

Synthetic and regenerated materials

Sipol lists high adhesion to both, for mixed-material shoe constructions.

Rod extrusion

PA 162/G granules are mainly used as raw material for extruding the rod cement.

Handling and dispersion

The PA 162-4.2 data sheet gives an indicative application temperature of 220 to 240 °C, and viscosity is measured at 232 °C, inside that window. Set the lasting machine within it and confirm the setting in trials.

Sipol recommends preliminary trials to approve PA 162, given the wide variety of materials used in footwear construction.

Packaging, storage, and regulatory status

Package sizes: Rod in 25 kg net cardboard boxes of 12 reels, around 1.67 kg each. PA 162/G granules in 25 kg bags with an aluminum film moisture barrier, 500 kg cardboard octabins with an inner PE liner, and 500 kg and 1000 kg big bags..

Storage: Rod (PA 162, PA 162-4.2) is stable for 18 months and granules (PA 162/G) for 24 months, unopened in the original packaging, in a cool, dry place protected from light. Material held at around 5 to 10 °C or below should stand at 15 to 20 °C for at least 24 hours before use.

Read the safety data sheet before handling.

Frequently asked questions

Will Technipol PA 162 run on a toe lasting machine with tracers?

Yes. Sipol designed Technipol PA 162 rod cement for automatic lasting machines and specifically to be used also on the new toe lasting machines equipped with tracers. The rod softens at 188 °C and measures 8.0 Pa·s at 232 °C. Sipol recommends preliminary trials on the actual shoe materials before approving it, given the range of constructions in use.

Which rod diameter of Technipol PA 162 should I order?

Technipol PA 162 comes as 3.9 ± 0.1 mm rod and as Technipol PA 162-4.2 at 4.2 ± 0.1 mm. Both have the same 188 °C softening point and 8.0 Pa·s at 232 °C, and both come on reels of around 1.67 kg, 12 to a 25 kg box. Order the diameter your lasting machine's feed is built for.

What is Technipol PA 162/G for?

Technipol PA 162/G is the granular form of the PA 162 polymer, mainly used as raw material for extruding the rod cement used by automatic lasting machines. It has the same 188 °C softening point and 8.0 Pa·s at 232 °C, comes in 25 kg bags, octabins and big bags, and keeps 24 months against 18 months for the finished rod.

How does Technipol PA 162 compare with Technipol PA 167?

Technipol PA 162 softens at 188 °C and measures 8.0 Pa·s at 232 °C. Technipol PA 167 softens at 172 °C and measures 3.5 Pa·s at 232 °C, a much more fluid melt. The PA 167 and PA 162-4.2 data sheets both give a 220 to 240 °C application window. Sipol names PA 162 specifically for toe lasting machines with tracers.

Can I get the TDS and SDS for Technipol PA 162?

Yes. We send the Technical Data Sheet (TDS) and Safety Data Sheet (SDS) on request, in the manufacturer's current revision. Use Request TDS or SDS above and tell us what your qualification review needs.

Related products

Technipol PA 167

Lasting rod at 172 °C and 3.5 Pa·s, in four versions.

Technipol PA/G

Footwear grade for automatic thermofolding machines, 110 °C softening point.

Technipol PA 2162

Same typical values in granules, positioned for automotive filters.

Where this grade fits

Copolyester and copolyamide hot melts

The Technipol and Technipol PA range by softening point and use.

Footwear hot-melt adhesives

Lasting rod, folding and shoe-assembly hot melts and how to choose between them.

Evaluating Technipol PA 162?

Tell us the system you are formulating and the property you need to hit. We will confirm the grade, send the data sheet, and ship a sample.